Change the combustion system
The middle and high-grade roller ring material include high manganese steel, alloy steel, etc with hardness of HRC50-55 and the wear-resistant layer thickness of 30-35mm, it can only be repaired by grinding instead of welding;
All steel welded construction, floating spindle, high chromium alloy wear resistant liner
Hard molding is generally 14 ~ 17%; Semi-hard molding is generally 16 ~ 19%; Soft plastic generally > 18%
Upper stage auger: high chromium alloys type doesn’t support welding; cast steel type supports welding
It is 500mm
Both the diameter and die head of small equipment such as VP35 are small, so it is incapable of producing large-size bricks
Usually 10,000 square meters is more suitable, the workshops are only part of the area, raw material storage and finished product storage areas must also be considered
The construction period is usually 6 months, with two technicians providing technical guidance and 20-50 labors
For the tunnel kiln, the length is 134 2m, and the size of kiln cart is 2 9*3 66*0 84m Coal feeding holes are arranged in the high-temperature section usually between 19th cart and 29th cart, about 24 columns Each column has 4 holes, total 96 holes or 4 or 5 holes staggered, total 108 holes
International Business:+86 181-8262-2677
Domestic Business:+86 156-1925-3978
Email address:info@brictec.com Website:www. brictec.com
Address:Room B501, R&D Building, ZTE Industrial Park, No. 10 Tangyan South Road, High-tech Zone, Xi'an City, Shaanxi Province, China.
Click on Map